HIGH LIGHT: IATF16949 involute spline shaft, modulus 2 involute spline shaft, 20CrMnTiH electric motor shaft
Shafts the shaft is (φ50-φ55) x (200-270) Motor Shafts the modulus in 2, The heat treatment process of the product is carburizing quenching, carburizing process is a very old process, in recent years, there is a high concentration of carburizing process.
Temper and crack occur during grinding
Causes: carburizing layer by grinding after the surface caused softening phenomenon, known as the grinding of tempering.
This is because the grinding process feed is too fast, grinding wheel hardness and particle size or speed selection is not appropriate, or the grinding process cooling is not sufficient, are easy to produce such defects.
This is because the heat of grinding softens the surface. The wear resistance of parts is reduced when tempering defects occur during grinding.